Precision Forming Technology of Large Superalloy Castings for Aircraft Engines von Baode Sun | ISBN 9789813362208

Precision Forming Technology of Large Superalloy Castings for Aircraft Engines

von Baode Sun, Jun Wang und Da Shu
Mitwirkende
Autor / AutorinBaode Sun
Autor / AutorinJun Wang
Autor / AutorinDa Shu
Buchcover Precision Forming Technology of Large Superalloy Castings for Aircraft Engines | Baode Sun | EAN 9789813362208 | ISBN 981-336-220-0 | ISBN 978-981-336-220-8

Precision Forming Technology of Large Superalloy Castings for Aircraft Engines

von Baode Sun, Jun Wang und Da Shu
Mitwirkende
Autor / AutorinBaode Sun
Autor / AutorinJun Wang
Autor / AutorinDa Shu

This book describes systematically the theory and technology of the precision forming of large, complex and thin-walled superalloy castings for aircraft engines, covering all the important basic aspects of the manufacturing process, including process design, wax pattern, ceramic molds, casting and solidification, heat treatment, repair casting and dimension precision control.

The correlation of casting defects, structural characteristics and performance of castings is revealed through a range of tests. It also discusses the latest technologies and advances in this field – such as imaging the solidification process by means of synchrotron radiography, 3D computerized tomography and reconstruction of microporosity defects, analysis and diagnosis of error sources for dimension over-tolerance and adjusted pressure casting technology – which are of particular interest. Providing essential insights, the book offers a valuable guide to the design and manufacture of superalloy casting parts for aircraft engines.